Sign In | Join Free | My enlightcorp.com |
|
Brand Name : YUHONG SPECIAL STEEL
Model Number : ASTM A335 P22 Alloy Stainless Steel Seamless Pipes
Certification : ISO,SGS,BV,ISO & SGS,ISO/CE/SGS
Place of Origin : CHINA
MOQ : 100KGS
Price : NEGOTIABLE
Payment Terms : L/C, T/T
Delivery Time : 20-80
Packaging Details : Ply-wooden Case /Iron Case/ Bundle with plastic Cap
OD : 10—600mm
Technique : Hot rolled
Specification : ASTM A335 P22 Alloy Stainless Steel Seamless Pipes
Surface Treatment : Black Painted
Package : Standard Seaworthy Package
Application : Boiler pipe, chemical fertilizer pipe, structure pipe
ASTM A335 P22 Alloy Steel Seamless Tubes Hot Rolled for Boiler
YUHONG is one of the biggest manufactures of stainless steel & duplex steel & alloy steel tubes and pipes in China.
1.Manufacture method: cold rolled, cold drawn, hot rolled.
2,material:P22
2.Standard:ASTM A335 p22
3.Size range: 12.7mm*1.2mm - 325mm*50mm
4.Delivery condition: normalized, normalized+tempered,Quenched+tempered
5.Payment terms: T/T 30%payment in advance, 70% T/T before shipment or by L/C
6.Packing: Export sea worthy package
7.END:<2" (60.3mm) Plain end;>2"(60.3mm) Bevelled end; Square cut;Plastic caps at both ends
8.Application:Structural use ,roofing, commercial use, household appliance, industry, family etc
9.Quality control:
a)Mill Test Certificate is supplied with shipment.
b)Third party inspection is highly welcomed.
P22 Pipe Chemical Requirements
Propriétés chimiques | |||||||||
---|---|---|---|---|---|---|---|---|---|
Carbone | Silicium | Manganèse | Phosphoreux | Soufre | Molybdène | Nickel | Chrome | Cuivre | Autres |
0.05-0.15 | 0,50 max | 0.30-0.60 | 0.025 | 0.025 | 0.87-1.13 | – | 1.90-2.60 | – | – |
P22 Pipe Mechanical Properties
Tensile Strength, MPa | Yield Strength, MPa | Elongation, % |
415 min | 205 min | 30 min |
ASTM A335 Gr P22 Equivalent Material
Désignation équivalente | |||||
---|---|---|---|---|---|
VACARME | FR | BS | NFA | ASTM | COMME MOI |
DIN 17175 Grade 10CrMo9-10 | EN 10CrMo9-10 Grade 10253 - 2 | NFA A 49-215 Grade TU 10 CD 9-10 | ASTM A335 Grade P22 | ASME SA 335 Grade P22 | UNI G3458 |
Heat Treatment Requirements
P5, P9, P11, and P22 | |||
Grade | Heat Treatment Type | Normalizing Temperature Range F [C] | Subcritical Annealing or Tempering Temperature Range F [C] |
P5 (b,c) | Full or Isothermal Anneal | ||
Normalize and Temper | 1250 [675] | ||
Subcritical Anneal (P5c only) | 1325 - 1375 [715 - 745] | ||
P9 | Full or Isothermal Anneal | ||
Normalize and Temper | 1250 [675] | ||
P11 | Full or Isothermal Anneal | ||
Normalize and Temper | 1200 [650] | ||
P22 | Full or Isothermal Anneal | ||
Normalize and Temper | 1250 [675] | ||
P91 | Normalize and Temper | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
Quench and Temper | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
Tensile Requirements
Seamless | ASTM A335 P5 | ASTM A335 P9 | ASTM A335 P11 | ASTM A335 P22 | ASTM A335 P91 |
Tensile Strength, min., psi | |||||
ksi | 60 | 60 | 60 | 60 | 85 |
MPa | 415 | 415 | 415 | 415 | 585 |
Yield Strength, min., psi | |||||
ksi | 30 | 30 | 30 | 30 | 60 |
MPa | 205 | 205 | 205 | 205 | 415 |
ASTM A335 Grade P22 pipes are commonly used in applications such as power generation, petrochemical plants, refineries, and other high-temperature and high-pressure environments where resistance to corrosion, high temperature, and stress are crucial.
![]() |