Sign In | Join Free | My enlightcorp.com
China Yuhong Group Co.,Ltd logo
Yuhong Group Co.,Ltd
Yuhong Holding Group Co.,LTD
Verified Supplier

14 Years

Home > Steel Flange >

ASTM B462 / ASME SB462 UNS N08020 Nickel Alloy 20 Superalloy Pipe Flange

Yuhong Group Co.,Ltd
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now

ASTM B462 / ASME SB462 UNS N08020 Nickel Alloy 20 Superalloy Pipe Flange

Brand Name : YUHONG

Model Number : ASTM B462 UNS N08020 Nickel Alloy 20 Superalloy Flange

Certification : API , ABS, DNV, GL , LR, NK

Place of Origin : CHINA

MOQ : 1PC

Payment Terms : L/C,T/T

Delivery Time : 7 DAYS

Packaging Details : Ply-wooden Case /Iron Case/ Bundle with plastic Cap

Product Name : Superalloy Pipe Flange

Standard : ASTM B462 / ASME SB462

Material : UNS N08020 Nickel Alloy 20

Size : 1/2"-120"

Process : Forged

Pressure : Class150/300/600/9001500/2500

Flange Face : RF/FF/RTJ

Type : Threaded Flange,Slip On Flange,socket Weld Flange,weld Neck Flange,LAP Joint Flange

Application : Petroleum,chemical,etc,fittings And Connection,beer

Contact Now

ASTM B462 / ASME SB462 UNS N08020 Nickel Alloy 20 Superalloy Pipe Flange

We are one of the biggest projects pipeline products supplier in China, Our products contain steel pipe/tube,fittings, flanges. With development more than 20 years, we have accumulated a great many clients all around the world and Yuhong products also won the great praise among the customers.

Alloy 20 will resist corrosion especially in those environments that contain chemicals like nitric acid, phosphoric acid, chlorides and sulfuric acid. Alloy 20 also has good mechanical properties at both ambient as well as elevated temperatures. Alloy 20 is often termed as a superalloy. ASTM B462/ ASME SB462 Uns N08020 Blind Flange has excellent resistance to general corrosion, pitting, and crevice corrosion in chemicals containing chlorides as well as in acidic medium or conditions that contain acidic solutions like sulfuric, phosphoric, and nitric acids.

Alloy 20 Forged and Plate Flange

ASTM B462 Alloy 20 Slip-On Flange
ASTM B462 Alloy 20 Threaded Flange
ASTM B462 Alloy 20 Weld Neck Flange
ASTM B462 Alloy 20 Socket Weld Flange
ASTM B462 Alloy 20 Blind Flange
ASTM B462 Alloy 20 Reducing Flange
ASTM B462 Alloy 20 Lap Joint Flange
ASTM B462 Alloy 20 Plate Flange
ASTM B462 Alloy 20 Orifice Flange
ASTM B462 Alloy 20 Forged Flange
ASTM B462 Alloy 20 Ring Type Joint Flange
ASTM B462 Alloy 20 Square Flange

Alloy 20 Flanges Equivalent Grades

STANDARD WERKSTOFF NR. UNS AFNOR EN
Alloy 20 2.4660 N08020 Z2NCUD31-20AZ NiCr20CuMo

Mechanical Properties

Alloy Tensile Strength, min. Yield Strength, min. Elongation, min. Reduction of Area, min.
ASTM B462 ksi MPa ksi MPa % %
UNS N08020 80 551 35 241 30.0 50.0

*All values shall be measured at room temperature.
*Alloy 20 flanges shall be supplied in stabilized-annealed condition.

Chemical Composition

Element Wt, %
Carbon [C] ≤0.07
Manganese [Mn] ≤2.00
Phosphorus [P] ≤0.045
Sulfur [S] ≤0.035
Silicon [Si] ≤1.00
Nickel [Ni] 32.00~38.00
Chromium [Cr] 19.00~21.00
Molybdenum [Mo] 2.00~3.00
Copper [Cu] 3.00~4.00
Niobium+Tantalum [Nb+Ta] 8xCarbon~1
Iron Remainder

*The tabulated values are abstracted from ASTM B462 Gr. UNS N08020.

ASME SB462 Alloy 20 Slip on Flange Vs DIN 2.4660 Weld Neck Flange
The ASME SB462 Alloy 20 Slip on Flange is slipped into the pipe and then the connection is made with the help of double weld- one on the backside of the flange and one in the front. Generally, the slip on flanges are more affordable than the weld neck flanges, but it can become expensive with the number of welding and inspections. Also, the strength of the slip on flange under any internal pressure is around 2/3rd, and fatigue strength is around 1/3rd of that of the weld neck flange

The DIN 2.4660 Weld Neck Flange is easily recognizable by the tapered hub which comes from the bolted connection to the pipe. The connection is made here with the help of but twelding, and that helps in preventing any type of turbulence at the joint. It also minimizes erosion and reduces restriction in the product flow. The alloy 20 weld neck flanges offer enhanced strength under different types of environments.

Application

  • Marine enviroments
  • Desalination systems
  • Flue gas desulfurization equipment
  • Reaction vessels for pharmaceutical production

ASTM B462 / ASME SB462 UNS N08020 Nickel Alloy 20 Superalloy Pipe Flange


Product Tags:

ASME SB462 Pipe Flange

      

Superalloy Pipe Flange

      

ASTM B462 Pipe Flange

      
Quality ASTM B462 / ASME SB462 UNS N08020 Nickel Alloy 20 Superalloy Pipe Flange for sale

ASTM B462 / ASME SB462 UNS N08020 Nickel Alloy 20 Superalloy Pipe Flange Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Yuhong Group Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)